Check your area ratio.
Christopher J. Nash
Mid-West Technical Support Engineer
Indium Corporation
Phone #: (315) 853-4900 x7521
Fax #: (315) 853-1000
www.indium.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ron Peeler
Sent: Friday, June 08, 2007 10:57 AM
To: [log in to unmask]
Subject: [TN] Insufficient Solder
Here is an age old question. Does anyone here have a sure fire way to
combat insufficient solder. I have tried all teh tecniques from what I know
of. These consist of changing stencil thicknesses, changing pastes,
re-training ops to IPC-610-D. I am at a lost. It seems that each operator
sees insufficient solder differently and it is almost an excuse from them to
keep busy and make added "touch up." I am almost ready to through the
category out the door b/c it is so subjective adn people are so fickle.
Any ideas out there?
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|