Richard,
I am certainly glad you didn't find the term "Insufficient Solder" in
any of the citations that you offered. I'm also glad that you're only
disturbed by the throw away line.
I have seen people identify many of the defects that you pointed to plus
dewetting, nonwetting, and minimum acceptable solder, as "insufficient
solder." My real message was that you need to be very careful when
putting an Inspector in charge of determining when product must be
repaired and even worse, when product lines must stop. Besides I think
that you could find each of those defects specified, while they might be
caused by insufficient solder, might also be caused by something other
than "insufficient solder."
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Monday, June 11, 2007 1:09 PM
To: TechNet E-Mail Forum; Glen Herzog
Subject: RE: [TN] Insufficient Solder
Boy, oh, boy, I have to take exception with the statement:
"Incidentally, I don't think that the term "Insufficient Solder" is in
either standard. I think that it is just a general term that we often
use without much definition."
The minimum amount of solder forming a fillet around the unsupported and
the plated-through-hole lead is clearly defined for each class in
section 6.1 and 6.2. The minimum amount of solder hole-fill is defined
for each class in section 6.3.2 in J-STD-001D The minimum heighth of the
heel fillet for gullwing leads is clearly defined for each class. See
section 7.6.7 and Table 7-7. The minimum endcap fillet for chip caps and
resistors is clearly defined for each class. See Table 7.4 The minimum
amount of LCC fill is clearly defined. See figure 7-6 and Table 7-6. The
minimum amount of solder required for MELF terminations is clearly
defined in Table 7-5.
And so on and so forth...
Anything not meeting the minimum is insufficient solder.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Monday, June 11, 2007 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] Insufficient Solder
Ron,
Your question, "Does anyone here have a sure fire way to combat
insufficient solder." apparently has two interpretations (1) how do I
get sufficient solder and (2) What should my inspectors do when there is
insufficient solder. I'll try to address the inspector issue.
Normally, inspectors do not cause rework. They have criteria from
J-STD-001 and ANSI/IPC-A-610. Based on that criteria they will
determine if an assembly passes or fails the criteria. Unless that
Inspector is quite experienced, a Quality Technician or Engineer, or a
Process Engineer determines what action must be taken. Often
"Insufficient Solder' is a process indicator. The process needs
improved, but the board does not need to be reworked.
Incidentally, I don't think that the term "Insufficient Solder" is in
either standard. I think that it is just a general term that we often
use without much definition.
Good Luck, Ron
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|