How about:
Increasing stencil thickness (and reduce apertures where more solder is
not needed).
Using a stepped stencil - only increase thickness for certain parts.
Solder preforms added by a pick and place machine to complement paste.
Additional paste added by a liquid dispensing machine if available.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg A. Owens
Sent: Friday, June 08, 2007 2:06 PM
To: [log in to unmask]
Subject: [TN] Solder Stencil - Insufficient Solder
Dear TechNetters:
Continuing with the theme of insufficient solder. Have a student with a
similar problem. They have a few SMT components that are very large (in
relation to the majority of others on the PCB). These larger components
then have insufficient solder necessitating too much touchup/rework to
be cost effective. Is there a way to increase the quantity of solder
paste being applied to these specific components using a stencil other
than increasing the aperture? Any other ideas?
Thanks,
Gregg Owens, MIT
Manufacturing Technology Training Center, Inc.
Mira Loma, CA 91752
Gregg
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|