TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 22 Jun 2007 16:07:44 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ron Peeler <[log in to unmask]>
Subject:
From:
Ron Peeler <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (108 lines)
I guess one of the questions is if the pitted area has the same layer of gold thickness as the regular area.  If not then premature "wear" in the pitted areas can occur.  Early failures in the field, etc.

Ronald D. Peeler Jr., B.S. IE 
Process Engineer 
SWEMCO 
Moorestown, NJ 08057 
Tel: (856).222.9900 ext. 31 
Cel: (484).948.0779 
Fax: (856).222.0700 
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ian Hanna
Sent: Friday, June 22, 2007 3:59 PM
To: [log in to unmask]
Subject: Re: [TN] Gold finger pitting


It's the nickel -- not the gold...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, June 22, 2007 3:53 PM
To: [log in to unmask]
Subject: [TN] Gold finger pitting

Please see the picture.  We believe the copper underneath the gold is
where the pitting occurs.  It appears fully plated with gold, even in
the pits.
It doesn't seem to meet the IPC-600 spec, but I was wondering what are
the potential problems this could cause.

________________________________

From: Steve Gregory [mailto:[log in to unmask]] 
Sent: June 22, 2007 1:49 PM
To: Genny Gibbard
Subject: RE: Gold finger pitting


Hi Genny!
 
It's up! Go to:
 
http://stevezeva.homestead.com/files/Pitted_Gold_Fingers.jpg
 
I don't know if I would accept it either. Is it the gold that's pitted,
or the copper beneath it? Or can you tell?
 
Have a good weekend!
 
Steve

________________________________

From: Genny Gibbard [mailto:[log in to unmask]] 
Sent: Friday, June 22, 2007 1:45 PM
To: Steve Gregory
Subject: Gold finger pitting



Steve could you please help me out here and post a pic? 
I need the learned response of Technetters. 
This does not appear to meet IPC, but I am not sure what the hazards of
letting it go thru would be. 
<<pitted gold fingers.pdf>> 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2