The shop I work for uses 3M Scotch Brand palters tape (#1280) for HASL gold protection and for plating operations. The operators must be careful to have clean hands wile handling the tape. If cleanliness is practiced, we have no problems with the tape.
Karl
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dan Slocum Jr.
Sent: Thursday, June 21, 2007 11:18 AM
To: [log in to unmask]
Subject: [BULK] [TN] Covering Selective Ni-Au features through HASL
Importance: Low
Has anyone had a great amount of success with any particular product? I
realize that kapton is probably most commonly used, but any specifics would
be appreciated (brand, etc.)
Regards,
Dan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|