Dave,
thanks for the reply. What detrimental effects should I be
worrying about if/when Nickel levels go above the stated maximum of
0.01% and at what point is this considered bad enough to dump the soldr
bath contents and start afresh? The machine suppliers tell me that even
treated stainless parts (chrome carbide?) still allow the nickel to
dissolve into the pot contents.
Regards
Nigel Burtt
Production Engineering Manager
Dolby Laboratories, Inc. - European HQ
Email: mailto:[log in to unmask]
Tel: +44 (0)1793 842132 [direct line with voicemail]
Fax: +44 (0)1793 842101
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you
are not the intended recipient, delete this message. If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|