I'm going waaaay back here but it sounds to me like there
may be an issue with the size of the great apes on the factory
floor. I recall having many problems on a paper-epoxy
single sided board where handling post assembly and before
test was causing components to be pushed through and so
lifting the land, track, solder joint and everything. These
were not small pads, either.
One cure for that was simply plating the hole, while not the
most graceful solution the added adhesion vastly reduced the
frequency and severity of damage. What I can't recall is if
we tried simply switching to FR4.
Yikes, I'm dating myself... Just guessing someone else in that
decision chain is my age...
--
Jeff Seeger Applied CAD Knowledge Inc
Chief Technical Officer Tyngsboro, MA 01879
jseeger "at" appliedcad "dot" com 978 649 9800
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|