TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roger Tingler <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Tingler <[log in to unmask]>
Date:
Thu, 31 May 2007 07:31:25 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (101 lines)
Terry, 

There are several products that has high thermal conductivity that would fit
your requirements 
 
We have used Thermagon-T-Lam/preg (Laird purchased Thermagon) and
Berqquist-Thermal clad for thermal management in multi-layer and FR4-hybrid
PCB constructions 
 
http://www.lairdtech.com/pages/catalogs/thermal.asp

http://www.bergquistcompany.com/thermal_substrates.cfm

Hope this helps, 

Regards,


Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
  540-752-5511x102
F:800-631-0856
  540-752-4832

E-mail: [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Kozlyk
Sent: Thursday, May 31, 2007 7:02 AM
To: [log in to unmask]
Subject: [TN] Conductive Cooling thru Pre-Prig material

Technetters;

 

I have a 6 layer PCB with about 8 HOT DPAK components. The tabs are
electrically hot so I cannot just draw the heat directly thru a copper fill
brought out to the edge of the PCB.

 

I need electrical isolation, BUT high thermal conductivity between 2
adjacent layers.

 

Can anyone recommend what material they have specified to be used for
pre-prig that conducted the heat to the adjacent layer?

 

Voltage max is about 50 volts so I could probably go down to 2 or 3 mil
pre-prig.

 

Nothing special about this PCB; about 5" x 5".

 

The fab houses I solicited for info still haven't replied so I am curious.

 

Any leads, products or websites would be appreciated.

 

Regards

TDK


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2