Hi Sly!
Laguna Seca? Now you're talking! That's one of my ol' stomping grounds
when I was out in California. I was part of the safety crew that worked
some of the big motorcycle races (AMA and FIM races) at Laguna and Sears
Point (now Infineon Raceway I think?).
Anyways welcome aboard!
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sylvain Kaufmann
Sent: Tuesday, May 29, 2007 2:49 AM
To: [log in to unmask]
Subject: Re: [TN] SAC/ENIG report
Hi Inge and other netters!
First, thank you Inge for the report and for your welcome.
Well, I didn't know how I would post my first message on TN, here I am!
No, i didn't think you are snob guys, but my forumphobia was stronger!
So, as said below, I'm a technician working for a small electronic
workshop (and would preferably battle with John on Laguna Seca) in a
small mountainy (and snowy this weekend) country and I'm new around
here; hello all and congratulations for the way you make this forum
live.
Have a nice day.
sly
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: lundi, 28. mai 2007 17:45
To: [log in to unmask]
Subject: Re: [TN] SAC/ENIG report
Welcome Sylvain - greetings from John Burjke - engineer (and would be
full time motorcycle racer) from Santa Clara
California......................
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Sunday, May 27, 2007 11:59 PM
To: [log in to unmask]
Subject: Re: [TN] SAC/ENIG report
Dear Sylvain,
I regret your bad experience from the 'other' forum. What on earth was
that forum? Sounds like being a snob's club. I feel upset. I promis
you, TechNet is far from that! All are welcome to participate in the
discussions, even doctors.
TechNet is a mix of professionals, lunatics, retireds, amateurs,
supervisors, presidents, designers, purchasers, brokers, consultants,
professors, students....all, but no posh snobs!
So, I'll send the report to you, and at the same time, I ask you to
shake hands with the TechNet gnus electronically. I'm sure you will get
a lot of welcome greetings.
I send parts of your mail to the forum, so that the guys can see there
is a new member. I'm sure you will contribute with good things yourself.
Welcome!
Inge
------------------------------------------------------------------------
---------------------------------
quoted:
-----Original Message-----
From: Sylvain Kaufmann [mailto:[log in to unmask]]
Sent: den 24 maj 2007 18:00
To: Hernefjord Ingemar
Subject: SAC/ENIG report
Dear Mister Hernefjord,
Sorry to take contact with you directly when we never met or talk
before.
I am a very little experienced (about 5 years) production technician and
I'm new by IPC's forums. I never worked for mass production and allways
had to manage high mix/low volume production processes and equipment in
a high mix/low volume country.
..............
.............
..............
I saw on IPC Technet forum that could maybe share a very complete report
on ENIG/SAC combination; may I, please, ask for one copy of this report?
I'm sorry to take your time like this, but as a newcomer I didn't want
to post on technet because I thought you could not appreciate a querry
like this from someone you never heard of. I have to admit, too, that I
have been traumatized on another forum, I won't name it, where I have
been "shot down" because I was not any doctor or metallurgist and my
questions were to low-level ones.
Thank you and sorry again for disturbing through your professionnal
e-mail.
Kindest regards.
S. Kaufmann
************************************************************
Sylvain Kaufmann
CERN / European organisation for nuclear research Site de Meyrin
1211 Geneva 23
Switzerland
Dpt: TS-DEM-WS (int mail J06600)
Phone: +41 22 767 37 02
Fax: +41 22 766 87 77
E-mail: [log in to unmask]
Web: www.cern.ch
http://ts-dep-dem.web.cern.ch/ts-dep-dem/
************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|