Rob,
If you plan to use fluxes beyond what is called out in J-Std-001D,
paragraph 3.3, for Mil work class 3, then you need to run the
qualification testing outlined in the standard.
I've run thru this process twice, and I'm about to do it a third time due
to equipment and material changes.
Costs between $5 - $10K to complete this qual process.
Needs to be done to validate your cleaning processes.
Good Luck.
Robert Coburn <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/22/2007 08:56 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Robert Coburn <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Mil assemblies & No Clean
Hi T'netters;
We are looking into moving all assembly requirements into one facility.
The current location performing MIL assembly will move to the commercial
assembly facility.
Here are the initial questions:
Does the Military accept a No Clean process?
Or must the process use water soluble flux?
TIA,
Rob
_________________________________________________________________
PC Magazine?s 2007 editors? choice for best Web mail?award-winning Windows
Live Hotmail.
http://imagine-windowslive.com/hotmail/?locale=en-us&ocid=TXT_TAGHM_migration_HM_mini_pcmag_0507
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|