TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 2 May 2007 14:44:29 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (314 lines)
Juan,

there are plenty of links in the archives, here's a couple:
http://www.datumdynamics.com/products/wave_solder_fixtures.php
http://www.ascenteceng.com/
http://www.dmipallet.com/
http://www.emcgti.com/products/productView.asp?id=6
http://www.pentagon-ems.com/

Good luck,

Ioan

-----Original Message-----
From: Rojas, Juan [mailto:[log in to unmask]]
Sent: Wednesday, May 02, 2007 2:20 PM
To: TechNet E-Mail Forum; Tempea, Ioan
Subject: RE: [TN] LeadFree - ICT FPY Benchmarking


I firmly believe it is from the wave.  Would you please elaborate more
on the masking carriers?

Best regards,
Juan Rojas | Sr. Test Engineer | Harman/Becker Automotive Systems |
office: (270) 598-4555 | www.harmanbecker.com
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Wednesday, May 02, 2007 9:42 AM
To: [log in to unmask]
Subject: Re: [TN] LeadFree - ICT FPY Benchmarking

Juan,

in case the experiment below shows the residue being the problem, you
will have to answer to this question: is it the SMT paste residue that
bothers you or the flux residue from wave?

If it is the SMT you might want to revise the PCB, for proper probe
acess. If your trouble is the waving, it is just a matter of using
masking carriers.

Regards,

Ioan

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Burke
Sent: Tuesday, May 01, 2007 4:34 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree - ICT FPY Benchmarking


Yes as a matter of fact.

Produce 2 small runs of product in 2 groups of 10.

It sounds like you are using a no clean flux so process one that way.

Process the second batch using the same manufacturers paste in a water
clean
version. If you haven't got a cleaner before you start arrange with a
local
contract house that has a water cleaner to drive the reflowed second
batch
straight there and throw them through their water washer.

Now you have 2 sets of 10 boards as a comparison to run testing trials
on
one of which should be "squeaky clean" which should eliminate or
incriminate
the flus residue question.

Have fun,

John
 
 
John Burke
 
(408) 515 4992

 BY the way when you say "oxidation" what is the board finish? Gold will
not
oxidise and silver oxide is conductive.
 
-----Original Message-----
From: Rojas, Juan [mailto:[log in to unmask]] 
Sent: Tuesday, May 01, 2007 1:06 PM
To: TechNet E-Mail Forum; John Burke
Subject: RE: [TN] LeadFree - ICT FPY Benchmarking

Thanks John,

Yes we are having what it appears to be typical contact problems (due to
residues like: flux, oxidation, etc.) But I can not prove this yet; even
when we re-test a failing board it passes without doing anything to it;
this is not sufficient to convince my fellow process engineer.
We also have a lot of problems with capacitor tests that fails
marginally it is a very unstable test (caps)I attribute it still to
residue but again it is very difficult to me to prove it.

Any ideas? Comments are welcome.

Best regards,
Juan Rojas | Sr. Test Engineer 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, May 01, 2007 3:00 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree - ICT FPY Benchmarking

Agreed, attention to detail is everything...

Juan, If you are having an issue with yield (which you have not stated)
how
does it compare with the leaded version?

John

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, May 01, 2007 12:09 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree - ICT FPY Benchmarking

Well, thank you. We certainly put a lot of effort into it. It is really
amazing what it takes to get better than 5 sigma.
Everything from pad design library, part type selection, DFMEA, type of
pwb material, surface finish, selection and qualification of solder
paste, process details, component vendor qualification, receiving
inspection procedures, process controls on reflow/paste
print/pickandplace/reflow/wavesolder, fixture DFMEA, etc., etc,.......  
When you think about it, all of the efforts put into getting a 99%
cumulative yield and maintaining it over time is a major task. Many are
doing it today, but it sure is not an easy thing to accomplish.

-----Original Message-----
From: Rojas, Juan [mailto:[log in to unmask]] 
Sent: Tuesday, May 01, 2007 1:54 PM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: RE: [TN] LeadFree - ICT FPY Benchmarking

Wow! you're really doing well.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, May 01, 2007 1:08 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree - ICT FPY Benchmarking

It should be around 99% or better. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rojas, Juan
Sent: Tuesday, May 01, 2007 11:36 AM
To: [log in to unmask]
Subject: [TN] LeadFree - ICT FPY Benchmarking

Hi Everyone,

 

Would you mind if you can share with me what a typical ICT FPY is?

 

For the following PCBA:

 

Pb-Free process

~300 Test points

Low Board complexity (~500 analog components)

Board size: 6 x 9 in

Single side board

Test pad size diameter 35 thou

 

A ball park number would be fine.

 

Best regards,

Juan Rojas, MITMB | Sr. Test Engineer | Harman/Becker Automotive Systems
| office: (270) 598-4555 | www.harmanbecker.com
<http://www.harmanbecker.com/harmanBecker/www_root/index2.jsp?language=U
S> 

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2