TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Fri, 11 May 2007 11:04:20 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (65 lines)
Hi Werner!

I once was foolish enough to have a flex circuit ENIG plated in the
flexible area.  The results were disastrous.  Of course, the problem
isn't the gold, it's the nickel.

But I haven't seen a similar problem with vias in rigid boards as of
yet.  Are Z-axis excursions going up due to material changes and or
process temperatures due to ROHS?

Wayne Thayer

>>> [log in to unmask] 5/11/2007 10:51 am >>>
Hi 'Netters,
I am coming across some horror stories with ENIG plating inside vias,
with 
the ENIG fracturing during solder-T excursions and then digging into
the ED-Cu 
causing stress concentrations and ED-Cu fracturing. My own fatigue
ductility 
testing of ED-Cu foil with ENIG plating shows much reduced fatigue
life. This 
is, of course of no consequence on a soldering pad, but inside the via,

particularly with the much higher solder-T's required for SAC, this
turns out to be a 
real problem.
I would appreciate hearing about other experiences, and how people are

handling this.

Werner



**************************************
 See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2