Technetters,
I would like to measure the oxidation of the solder spheres in solder
paste. I do not have an Auger or XPS. Now I know that ACI (EMPF) was
selling a device at one time that looked at solder paste quality on the
stencil. I am not referring to that equipment. I seem to recall there
was a Japanese piece of equipment that might have been something like a
SERA tester that claimed to be able to do this. I was wondering if
anyone on this forum had ever used it/checked it out? Or did it never
hit North American shores because of potential patent conflict with the
SERA tester? Any leads would be appreciated.
Regards,
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|