Hi Joe,
Sorry to say their is an epidemic of of failing laptops.
The Danish government is going after Apple, there is a class action against
Sony, I also heard about problems with HP and Dell...and to my knowledge, it is
all SJ failures.
I do not know whether it is LF or laptops getting smaller and with more
functionality and running hot—most likley some combination. I have ssen pictures of
people using C-clamps on laptop housings to be able to start their laptops—
putting pressure on the SJ fracture surfaces to make electrical contact.
It seems, DfR has never been heard of by this people.
However, your laptop takes the cake for customer...on the other hand, I have
heard of DOA's right out of the box at distribution centers.
Werner
**************************************
See what's free at http://www.aol.com.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|