Steve,
In my opinion , to make things simple in the beginning, and to avoid big
expenses, maybe your client must see that your reflow profile in the failed
locations is the correct one and similar to the profile on other locations
where there are no failures.
This is in order to show that you established the correct one for the
assembly, and for the parts in general.
(You know of course how to do it with local thermocouples)
If the failure appeared suddenly after having had good results before, look
for a change (component make or manufacturer) or circuit change ( artwork or
manufacturer).
If it is the first time you manufacture these circuits, and your profile and
stencil are correct as required by the component manufacturer in his
appliccation notes, the client can not pretend that your work is not
correct. After all, you are ASSEMBLING.
However, in order to correct the problem, if you decide to use a laboratory,
you should decide what relevant information you need , and this is where the
expert comes in.
Gaby
----- Original Message -----
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 30, 2007 11:24 PM
Subject: Re: [TN] Solder Joint Analysis Lab Recommendations?
> Hi Steve,
> Most commercial labs will do a very good job determining whether what you
> sent tem meets whatever spec is applicable. In most cases, they will not
> do
> interpretive work or root cause analysis.
> Excellent labs are Robisan, Microtek, Trace, and others—typically, the
> best
> are rather active within the IPC.
> For interpretive work or root cause analysis you need a consultant like
> me.
>
>
>
> Werner
>
>
>
> **************************************
> See what's free at http://www.aol.com.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|