There is a couple of companies that just do that due to the fact
that many components come with Tin only. Adding the lead avoids tin
whiskers.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Lamkin
Sent: Friday, May 18, 2007 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] Using up old components?
Replating the leads is unlikely to happen, for what a few reels cost
compared to all the hassle & cost of doing that does not really make it
worth it, also it's something we have never had done here so wouldn't
know where to start.
Thanks for the suggestion anyway,
Matthew Lamkin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dehoyos, Ramon
Sent: 18 May 2007 15:20
To: [log in to unmask]
Subject: Re: [TN] Using up old components?
replate the leads. If the leads replate, the diodes should still
be good.
Ramon
------------------------------------------------------------------------
------------------------------------------------------------------------
----
This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender on the telephone number +44-(0)1282-717171 or via
email return. Unless expressly stated otherwise, and subject to the
disclaimer below, this email does not form part of a legally binding
contract or agreement between the recipient and Protec Fire Detection
Plc. (registered no. 1170489). Registered Office: Churchill Way. Nelson.
BB9 6RT. Lancashire. United Kingdom.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorised alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Protec Fire
Detection Plc. makes no warranty as to accuracy or completeness. In
particular, Protec Fire Detection Plc. does not accept responsibility
for changes made to this email after it was sent. Any opinions or
recommendations expressed herein are solely those of the author.
------------------------------------------------------------------------
------------------------------------------------------------------------
----
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|