Good afternoon from Spain,
In a lot of PCA’s, we have detected several cases of discontinuities in the
inner layers –confirmed by microsections-
We would like to test the rest of the lot in accordance with the method 2.6.6
of IPC-TM-650, but this method doesn’t specify the temp ramp to pass from a
step to the following. Can you help us?
Thank you.
Juan
---------------------------------------------------