Hi,
You wrote that you use FCT SN100C since 1 year, we usually use it in our product but since 1 month we found some blow hole and void in our SMD solder joint, we use immersion tin plating. We spoke with their guru's but we are unable to find any reason for that. Those blow hole and voids are most of the times on LED with gold plating, do you have some ideas for us to solve our problem??
Thank You
Yannick
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]]De la part de Miguel Vallejo
Envoyé : 30 avril, 2007 18:21
À : [log in to unmask]
Objet : Re: [TN] SN100C vs. SAC305
I've been using FCT SN100C for both SMT and TH. I started using this alloy
since May 06. I've run around 30K boards, since, with no problems. Once
dialed-in, the process is very stable, and results very predictable. What I
love the most about this alloy is that the appearance is very similar to the
leaded solder, so there is no need for second criteria for acceptability.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Monday, April 30, 2007 11:42 AM
To: [log in to unmask]
Subject: [TN] SN100C vs. SAC305
Dear Technos,
I need to know how is this combat evolving. This topic has been brought up
several times, but things change fast right now and there must be more
empirical data on the matter.
What I know regarding the 2 materials can be summarized:
* Pro SN100C: cheaper, better looking, eats less copper in the TH
* One major unknown - the Reliability: SN100C is not available in
solder paste format, therefore the boards would have SAC SMT joints and
SN100C TH joints. This means 2 different materials and since we don't know
how reliable a board with only one material is, should we risk introducing
an extra variable?
I would like to know what your take is. Does anybody mixes the 2 materials?
Any reliability testing done? How long have you been doing it and do you see
RMAs?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|