Terry,
There are several products that has high thermal conductivity that would fit
your requirements
We have used Thermagon-T-Lam/preg (Laird purchased Thermagon) and
Berqquist-Thermal clad for thermal management in multi-layer and FR4-hybrid
PCB constructions
http://www.lairdtech.com/pages/catalogs/thermal.asp
http://www.bergquistcompany.com/thermal_substrates.cfm
Hope this helps,
Regards,
Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
540-752-5511x102
F:800-631-0856
540-752-4832
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Kozlyk
Sent: Thursday, May 31, 2007 7:02 AM
To: [log in to unmask]
Subject: [TN] Conductive Cooling thru Pre-Prig material
Technetters;
I have a 6 layer PCB with about 8 HOT DPAK components. The tabs are
electrically hot so I cannot just draw the heat directly thru a copper fill
brought out to the edge of the PCB.
I need electrical isolation, BUT high thermal conductivity between 2
adjacent layers.
Can anyone recommend what material they have specified to be used for
pre-prig that conducted the heat to the adjacent layer?
Voltage max is about 50 volts so I could probably go down to 2 or 3 mil
pre-prig.
Nothing special about this PCB; about 5" x 5".
The fab houses I solicited for info still haven't replied so I am curious.
Any leads, products or websites would be appreciated.
Regards
TDK
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|