Terry
Has the assembly been cleaned properly? Paralene really does not take
to no-clean assemblies.
I would be very wary of the comment that there is uneven coating
thickness - Paralene is deposited onto all surfaces in a vacuum
chamber, ever so thin.
Kindest regards,
Graham Naisbitt
Gen3 Systems Limited
[log in to unmask]
On 30 May 2007, at 13:45, Terry Quinn wrote:
> Does anyone in this group have experience with variations in the
> appearance
> of parylene coating? Our vendor is applying parylene on a small
> PCB. Most of
> the boards still exhibit the glossy finish of the original board
> mask but we see
> some units that have a distinctly dull or matte finish. Sometimes
> it is limited
> to one end or even a corner of the board. The vendor reports that
> this
> reflects a slightly thicker deposition of the parylene coating and
> is not a cause
> for concern. Can anyone confirm this, or are there other ideas
> that might
> explain this condition? Thanks for your help.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|