TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Mon, 28 May 2007 09:19:56 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (130 lines)
Sylvain,
Yes, Inge speaks for us all on the welcome and explaining the tenor of
the forum.  Even though some have PhDs, we remember is also stands for
"pile high and deeper" and we are not talking about sweet smelling
fertilizer either!

We do correct each other, but certainly from my ten years of experience,
usually in a proper or joking manner, if we know the writer well enough.

Welcome aboard.
Bev
RIM

PS I am a GUY, not of the female persuasion.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Monday, May 28, 2007 2:59 AM
To: [log in to unmask]
Subject: Re: [TN] SAC/ENIG report

Dear Sylvain,

I regret your bad experience from the 'other' forum. What on earth was
that forum? Sounds like being a snob's club. I feel upset.  I promis
you, TechNet is far from that! All are welcome to participate in the
discussions, even doctors.

TechNet is a mix of professionals, lunatics, retireds, amateurs,
supervisors, presidents, designers, purchasers, brokers, consultants,
professors, students....all, but no posh snobs!

So, I'll send the report to you, and at the same time, I ask you to
shake hands with the TechNet gnus electronically. I'm sure you will get
a lot of welcome greetings.

I send parts of your mail to the forum, so that the guys can see there
is a new member. I'm sure you will contribute with good things yourself.
Welcome!

Inge

------------------------------------------------------------------------
---------------------------------

quoted:

 

-----Original Message-----
From: Sylvain Kaufmann [mailto:[log in to unmask]] 
Sent: den 24 maj 2007 18:00
To: Hernefjord Ingemar
Subject: SAC/ENIG report

Dear Mister Hernefjord,
Sorry to take contact with you directly when we never met or talk
before.

I am a very little experienced (about 5 years) production technician and
I'm new by IPC's forums. I never worked for mass production and allways
had to manage high mix/low volume production processes and equipment in
a high mix/low volume country.

..............
.............
..............

I saw on IPC Technet forum that could maybe share a very complete report
on ENIG/SAC combination; may I, please, ask for one copy of this report?

I'm sorry to take your time like this, but as a newcomer I didn't want
to post on technet because I thought you could not appreciate a querry
like this from someone you never heard of. I have to admit, too, that I
have been traumatized on another forum, I won't name it, where I have
been "shot down" because I was not any doctor or metallurgist and my
questions were to low-level ones.

Thank you and sorry again for disturbing through your professionnal
e-mail.

Kindest regards.

S. Kaufmann

************************************************************
Sylvain Kaufmann
CERN / European organisation for nuclear research Site de Meyrin
1211 Geneva 23
Switzerland
Dpt: TS-DEM-WS (int mail J06600)
Phone: +41 22 767 37 02
Fax: +41 22 766 87 77
E-mail: [log in to unmask]
Web: www.cern.ch
http://ts-dep-dem.web.cern.ch/ts-dep-dem/
************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2