TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Steve Gregory <[log in to unmask]>
Date:
Thu, 24 May 2007 10:27:12 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (110 lines)
My guess is that the TSOP packages do have Alloy 42 lead
 Steve,



My guess is that the TSOP packages do have Alloy 42 leads and that you

may be seeing a failure that has gotten the name "Double Reflow"  I hate

that name almost as much as I hate the name "Black pad".  What do the

solder fillets look like on your TSOP packages?  If they look good but

your testing is indicating an intermittent and you can pass test by

pushing down on a TSOP lead I think you most likely have a brittle

interface solder joint fracture.  It will look like a perfect surface

mount solder joint with nice feathered solder fillets like it is wet

well to the PCB pad, and it probably was when it was formed.  However,

then the temperature is elevated and there is any mechanical stress the

solder joint can facture at the IMC bulk solder interface.  You won't be

able to see the fracture unless you view it at a low angle under high

magnification.  The "Double Reflow" name was coined by IBM Austin back

in 1979 presentation at NEPCON.  They called it "Double Reflow" because

their surface mount solder joints look great after surface mount reflow

soldering but failed (fractured) after the boards were wave soldered

(i.e., failed at the second reflow).  I've attached their NEPCON paper

as well as one we did describing a solder joint fracture we had using

QFPs with Alloy 42 leads.  We also saw similar failures on another

product on corner leads after the initial surface mount reflow.  Those

failures occurred during the first reflow and had nothing to do with

double reflow.  The solder joint fractures occurred on corner leads

during the surface mount reflow cooling process.



Regards, 

George 

George M. Wenger 

Senior Principle FMA / Reliability Engineer 

Wireless network Solutions 

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531

[log in to unmask] 





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory

Sent: Thursday, May 24, 2007 8:45 AM

To: [log in to unmask]

Subject: [TN] Silver Embrittlement?



Mornin' all!

 

I know this subject has been talked about before, but my memory is

getting rusty. I was wondering if it was possible to get solder joint

embrittlement on a board that has immersion silver finish and components

that have a flash gold finish? As you might have guessed, it's those

pesky Samtec SMT connectors...

 

We're experiencing another issue on that board as well. We're seeing

solder joint problems with some TSOP-66 DDR SDRAM that are on the

topside of the board. They're arranged close around two XILINX 1152-ball

BGA's that get very hot when the assembly is under power. Both BGA's

have large finned heatsinks mounted to the top of them. The BGA's get so

hot that if you power the board up without the heatsinks, and touch one

of the BGA's, you will burn your finger. There have been some cases that

during testing the board will fail and the failure points to one of the

SDRAM TSOP's. If you take something like the end of a wooden Q-Tip and

press on a suspect lead, the board passes test. The solder joint looks

fine upon initial inspection, but there's obviously an open connection.

I remember at one time TSOP leadframe material used to be made of

Alloy-42, is that still the case? These are parts from Micron

(MT46V16M16TG-6T), and I haven't yet found what the leadframes are made

of. I'm wondering if the stiffness of the leads may be contributing to

the solder joint failures that we're seeing. My theory is that because

the BGA's run so hot, they heat the PCB and cause board to expand in the

area around them (where the SDRAM are mounted).

If the leads on the SDRAM are stiff and non-compliant, the solder joints

might fracture.

 

Crazy theory I know, but I'm trying to figure what's going on with these

boards...

 

Steve Gregory 

	



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2