TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 23 May 2007 15:44:23 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (101 lines)
Were your recent meals this day Liquidous and Liquorous ?
Inge 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: den 23 maj 2007 15:36
To: [log in to unmask]
Subject: Re: [TN] Definition of Eutectic Solder

Hi Werner! Here is the definition from the American Society for Metals
(ASM) Metals Handbook, 2nd Edition:

"Eutectic. (1) An isothermal reversible reaction in which a liquid
solution is converted into two or more intimately mixed solids on
cooling, the number of solids formed being the same as the number of
components in the system"

Now, your definition is perfectly correct too and I agree with it. 
However, using the terms Liquidus and Solidus are necessary in the
definition. Most folks struggle a bit  with the terms Liquidus or
Solidus and I didn't want to get too deep in the metallurgy (Mr. Pauls
has such a hard time understanding metals and the English language in
general  (if folks haven't noticed,  Doug and I are making fun of each
other today). 

Lots of fun metallurgy discussions to start the day! Very cool.

Dave



Werner Engelmaier <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/23/2007 08:03 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Definition of Eutectic Solder






Hi Dave,
Sorry, I must disagree; your definition of "1) Eutectic: when a metal 
alloy 
transforms from a liquid state into a
single solid state" is wrong.
A eutectic alloy composition is by definition that composition where the

alloy's Solidus and Liquidus temperatures coincide and having the lowest

melting 
temperature among all other alloy compositions of the same materials.

Werner



**************************************
 See what's free at http://www.aol.com.


-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2