TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Mon, 21 May 2007 17:09:16 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (386 lines)
Sorry, Dewey, you misunderstood. You had to smoke the pot to imagine 
there was an improvement.

Believe it or not, in the very early days (early 1950s) of printed 
circuits, before Circuitape/Brady/Bishop brought out adhesive draughting 
aids, we drew the pattern in Indian ink on aluminium-reinforced 
cartridge paper (those were the days, my friend -- I think that may make 
a good song title!). I draughted along the orthogonal axes + 45° but a 
colleague always used a compass for wide radius bends because he 
believed the electrons would follow the track better without the 45° 
corners!!!

In those days, we used offset printing and while the ink was still wet, 
we sprinkled the board with a dark red powder (dragon's blood) which 
adhered to the wet ink. This was then heated and the powder melted to a 
pitch-like consistency. That was our etch resist! Anyone else remeber 
this "technology"?

Brian

Whittaker, Dewey (EHCOE) wrote:
> Back in the 70s, it was a highly held belief that if you pot the
> electronics, there was a great improvement in the clarity and depth of
> the music.
> Dewey
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Michael Kirschner
> Sent: Sunday, May 20, 2007 2:02 PM
> To: [log in to unmask]
> Subject: Re: [TN] Friday TechnoTopic
> 
> Heh heh...
> 
> It's all to feed, and thereby make $ off, the terrible disease called
> "audiophiliosis"...some friends of mine have it...spent tens of
> thousands of
> dollars on spectacular equipment and whiz-bang cables to listen to
> cassette
> tapes of Grateful Dead concerts...
> 
> ;o)
> 
> Mike
> 
> On Sat, 19 May 2007 10:50:39 +0300, Brian Ellis <[log in to unmask]> wrote:
> 
>> No, but it's great for 78s! :-)
>>
>> Brian
>>
>> John Burke wrote:
>>> Would it improve the sound on my 8 track??
>>>
>>> John...................8-)
>>>
>>>
>>>
>>> John Burke
>>>
>>> (408) 515 4992
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Fowler
>>> Sent: Friday, May 18, 2007 10:58 AM
>>> To: [log in to unmask]
>>> Subject: Re: [TN] Friday TechnoTopic
>>>
>>> They do have the amplifier built into the speakers.   I saw some
> about 8
>>> years ago, sounded nice, and were good and heavy.
>>>
>>> Then you can get into the copper crystalline signal cables, which are
>>> just as expensive as the speaker wires.
>>>
>>> It's all about the money...
>>>
>>> david
>>>
>>> Hogg, Blair K. wrote:
>>>> I wonder why someone doesn't just put the amplifier at the speaker
>>>> itself, then run line level audio through shielded cables to each
>>>> amplifier. Probably too much chance of em noise affecting the
> signal.
>>>> Could always go digital to the speaker, then turn it into audio
> signals
>>>> driving the voice coil. I think that is how it is done on some
>>>> automotive systems.
>>>>
>>>> -----Original Message-----
>>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
>>>> Sent: Thursday, May 17, 2007 9:27 PM
>>>> To: [log in to unmask]
>>>> Subject: Re: [TN] Friday TechnoTopic
>>>>
>>>> The world is full of nonsense. A friend of mine bought water cooled
>>>> speaker cables with pure gold connectors. That cable, I assure,
> could
>>>> supply current to a whole block in Santa Domingo. Myself, have an
>>>> ordinary "room cord" like the one you use for your desk lamp, this
> one
>>>> 15 feet long wire feeds a 800 W bass speaker. The loss in the wire
> is so
>>>> low, that it's neglectable, and the distortion would noone hear when
> the
>>>> bookshelves vibrate and you feel the thunder through the chair's
> legs. I
>>>> prefer to listen to the music, not to look at the music via a
>>>> oscilloscope and a spectrum analyzer.
>>>> Inge
>>>>
>>>> ----- Original Message -----
>>>> From: "Graham Collins" <[log in to unmask]>
>>>> To: <[log in to unmask]>
>>>> Sent: Friday, May 18, 2007 7:21 AM
>>>> Subject: Re: [TN] Friday TechnoTopic
>>>>
>>>>
>>>>
>>>>> Ha!  I'm guessing that wasn't a blind test.  How would that short
>>>>>
>>>> piece
>>>>
>>>>> of wire impact audio performance?  It's connecting a household plug
>>>>> socket, through the house wiring (of dubious quality if it's Inge's
>>>>> house...) and the power grid...  and has a transformer on the other
>>>>> side, presumably.
>>>>>
>>>>> I'm guessing this is along the lines of the speaker wire a sales
> guy
>>>>> tried to sell me one time.  It was 12 gage wire (overkill, but OK),
>>>>>
>>>> but
>>>>
>>>>> he was very earnest in telling me that the wire was formed such
> that
>>>> it
>>>>
>>>>> was optimized for electron flow in one particular direction...
>>>>>
>>>>> I'm thinking it's only applied to the AC power cord because
> anything
>>>>> more complicated would not emerge functional.  Component failures
>>>>>
>>>> aside,
>>>>
>>>>> what would that do to solder joints???
>>>>>
>>>>> regards,
>>>>>
>>>>> Graham Collins
>>>>> Process Engineer,
>>>>> L-3 Communications Electronic Systems Inc.
>>>>> Halifax
>>>>> (902) 873-2000 ext 6215
>>>>>
>>>>>
>>>>>>>> [log in to unmask] 05/17/07 10:37PM >>>
>>>>>>>>
>>>>> There is a process in High End Audio which purports to enhance
>>>>> equipment performance ,  called CryoTreatment.
>>>>>
>>>>> In this process the audio gear is subjected to a ramp down to -281F
>>>>>
>>>> (or
>>>>
>>>>> cooler, but not below -320F), followed by a soak of 20 to 40 hours,
>>>>> followed by a specific warm-up cycle back to R/T.
>>>>>
>>>>> It is postulated  that the technical  explanation for the enormous
>>>>> listening benefits  of the process is a re-arrangement or
> refinement
>>>> of
>>>>
>>>>> the crystal structure of the conductor metals. The effect is so
>>>>>
>>>> powerful
>>>>
>>>>> that objective listeners reported  a significant improvement in
> audio
>>>>> quality when the AC power cord for a preamp was so treated.  I
> doubt
>>>> my
>>>>
>>>>> aging ears are responsive to subtleties of this nature.
>>>>>
>>>>> Anybody care to estimate how an electronic assembly, surface-mount
> or
>>>>> otherwise, including  semiconductor devices, would fare thru  this
>>>>> process?
>>>>>
>>>>> Tom Stearns
>>>>> 3 Brander Court
>>>>> Nashua, NH
>>>>> 03063
>>>>>
>>>>> ---------------------------------------------------
>>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>>> To unsubscribe, send a message to [log in to unmask] with following
> text
>>>>> in
>>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>>> To temporarily halt or (re-start) delivery of Technet send e-mail
> to
>>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>>> [log in to unmask]: SET Technet Digest
>>>>> Search the archives of previous posts at:
>>>>> http://listserv.ipc.org/archives
>>>>> Please visit IPC web site
>>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>>> information, or contact Keach Sasamori at [log in to unmask] or
>>>>>
>>>> 847-615-7100
>>>>
>>>>> ext.2815
>>>>> -----------------------------------------------------
>>>>>
>>>>> ---------------------------------------------------
>>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>>> To unsubscribe, send a message to [log in to unmask] with following
> text
>>>> in
>>>>
>>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>>> To temporarily halt or (re-start) delivery of Technet send e-mail
> to
>>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>>> [log in to unmask]: SET Technet Digest
>>>>> Search the archives of previous posts at:
>>>>>
>>>> http://listserv.ipc.org/archives
>>>>
>>>>> Please visit IPC web site
>>>>>
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>>
>>>>> for additional information, or contact Keach Sasamori at
>>>>>
>>>> [log in to unmask] or
>>>>
>>>>> 847-615-7100 ext.2815
>>>>> -----------------------------------------------------
>>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following
> text
>>>> in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
>>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
>>>> ext.2815
>>>> -----------------------------------------------------
>>>>
>>>> *******************************************************************
>>>> This email and any files transmitted with it are confidential and
>>>> intended solely for the use of the individual or entity to whom they
>>>> are addressed. If you have received this email in error please
> notify
>>>> the system manager.
>>>>
>>>> This footnote also confirms that this email message has been swept
>>>> for the presence of computer viruses.
>>>>
>>>> www.Hubbell.com - Hubbell Incorporated
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following
> text in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>> for additional information, or contact Keach Sasamori at
> [log in to unmask] or
>>> 847-615-7100 ext.2815
>>>> -----------------------------------------------------
>>>>
>>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following
> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>> for additional information, or contact Keach Sasamori at
> [log in to unmask] or
>>> 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following
> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information,
> or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or
> 847-615-7100 ext.2815
>> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2