replate the leads. If the leads replate, the diodes should still
be good.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Lamkin
Sent: Friday, May 18, 2007 6:55 AM
To: [log in to unmask]
Subject: [TN] Using up old components?
Hello Technetters, it's a while since I have been here..
(I only ask here because Steve woke up & popped into the DesignerNet
forum reminding me about here :-)
I have been looking into our stocked components to improve my PCB
program's libraries to match what we stock etc.
I am coming across several components that we appear to have many
thousands of, yet are little used ("that" buyer no longer works for us -
lol) I.E. we have a BAV99 SOT23 diode that was purchased in 1992, 94,
94.
(it is used on a single board - only a few a year)
These are sat on a shelf, on the reel in a black anti static bag.
No air conditioning/humidity control etc.
Pulling the first diode off the reel & using a jewellers eyeglass I can
see that the legs look a little brown (tarnished).
I'm interested in what others do about this type of situation, do you
have a policy on using old components?
Do tarnished legs cause big problems soldering with lead free solder?
Thank you,
Matthew Lamkin.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|