You are mixing terms a little bit.
Soldermask is an epoxy (the green stuff)
HASL is metal, levelled with hot air
Anyway, we have been using the method
you describe to let the soldermask flow
up onto the via pads, but not into the hole,
So the soldermask clearance is "drill size
plus tolerance". The .15 is a good number
We haven't expereinced ANY fab or assy
problems using tis method.
BTW,
I invented a new name for these last week
when we were at the CID+ training:
"PONCHO VIA"
Jbro
On 5/31/07, Sanchez-Benavides, Erika <[log in to unmask]>
wrote:
>
> Hi!
>
> Due to the wave soldering process for PTH components, our assembly
> process guideline
> indicate to cover vias with soldermask in those areas.
> But as you know, Plated thru hole vias covered with soldermask on both
> sides with HASL
> solder or other manufacturing chemicals might be clogged in the vias and
> out-gas (blow out)
> during assembly or remain in the hole and corroid the copping in the
> via.
>
> There are two suggestions from our PCB suppliers:
>
> Resolution1: PCB supplier to add a clearance to the soldermask: (drill
> size plus.15mm).
> With this option, we are not going to have the via covered, but
> I am not sure if this is enough
> to avoid problems (pearls, solder passing through the via...)
> during wave soldering process.
>
> Resolution2: PCB supplier will tent the vias on both sides by adding a
> barrel relief to prevent their
> assembly problems.
>
> In your opinion, what would be the best option? Is there an alternative
> option you may see?
>
> Thank you very much in advance,
>
> Erika E. Sanchez
> Siemens VDO
> Guadalajara Development Center
> E-Mail: [log in to unmask]
> Internet: http://www.siemensvdo.com
>
>
>
---------------------------------------------------------------------------------
> DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL)
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
> E-mail Archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional
information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
>
>
---------------------------------------------------------------------------------
>
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
---------------------------------------------------------------------------------
"This e-mail message is intended only for the use of the intended
recipient(s).
The information contained therein may be confidential or privileged, and
its disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to its
sender at the above address and destroy it."
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|