DESIGNERCOUNCIL Archives

May 2007

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
DesignerCouncil <[log in to unmask]>
Subject:
From:
Gary Bremer <[log in to unmask]>
Date:
Tue, 29 May 2007 20:29:00 -0700
Content-Type:
text/plain; format=flowed
X-To:
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, Gary Bremer <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Where is it stated that the conductive pattern can not have any exposed 
copper on the vertical surfaces?  Is that any empirical data that supports a 
failure mode if there is exposed copper on the vertical surfaces of a 
conductive pattern? I have searched MIL-STD-2000, NASA-STD-8739-2 and 
NASA-STD-8739-3 but can only find that it is allowed. Where I work those 
with PhD's worry about exposed copper on the vertical edges of the 
conductive patterns and are scared to allow to move forward because of 
possible failure modes with a deep space launch. For my limited knowledge of 
metallurgy: after copper is exposed to moisture and oxygen, corrosion takes 
place only on the surface and does not migrate any further. I do have access 
to NHB5300 to see if exposed copper was not allowed.


Gary Bremer

_________________________________________________________________
PC Magazine’s 2007 editors’ choice for best Web mail—award-winning Windows 
Live Hotmail. 
http://imagine-windowslive.com/hotmail/?locale=en-us&ocid=TXT_TAGHM_migration_HM_mini_pcmag_0507

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2