Is it the board or the BGA warping.
****************************************
New address & phone numbers below
Guy Ramsey
R&D Assembly
1660 East Race Street
Allentown PA 18109-9580
(610) 443-2299
FAX (610) 443-1622
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ron Peeler
Sent: Thursday, April 26, 2007 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Bev,
You are completely right. This product that I have been "baptized" into has
been a 4 year terror. I am probably the 8th set of eyes to look at it. I
have seemed to make the most progress but that doesn't mean a thing. All I
do know is that the design is not good, the parts are obsolete and the board
is already being produced in a new generation build, so basically I am stuck
with what I have. Even though scrap is high on this board, they just want
to pump them out till they fizzle out. So I am stuck with trying to find a
reliable way to solder these BGA's when in 4 years they haven't been able to
on this board. I know that the warping on the board is causing the issue in
conjunction with the uneveness of the BGA package, neither of which can be
changed.
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, April 25, 2007 4:58 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Ron,
The problem right now is you see an effect and you do not know the cause.
It could be that the board and/or component warps and you have opens. It
could be that you have a head-in-pillow situation. It could be that you
have internal component opens. It could be that you have cracked solder
joints. You have to figure out which it is before you try to apply a
remedy.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ron Peeler
Sent: Wednesday, April 25, 2007 4:38 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Don't try me I just might ask you that...
:)
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: Wayne Thayer [mailto:[log in to unmask]]
Sent: Wednesday, April 25, 2007 4:35 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Hi Ron!
I think most people solve this problem by making sure the board and BGA are
planar during the process, and that the solder paste is thick enough to make
up the difference. Then you have the "collapse" process working for you
too.
Weights can be used but are painful--last resort. They absorb heat, messing
up the solder profile, and need to be fixtured so they don't fall off during
reflow.
Next you are likely to ask for a rule of thumb for the pressure supportable
by the solder surface tension and the compression of the solder balls which
ensues. I don't know that--I just try weights until it works.
Wayne Thayer
>>> [log in to unmask] 4/25/2007 4:23:12 pm >>>
Hello TechNet
I was wondering is there anything in the industry that is used to weigh
BGA's down? We are having an issue @ our shop with BGA's not soldering
effectively to one of our boards. Currently we have a board that is suppose
to go through a boot process, however it has problems doing so. The issue
is resolved when you press down in the middle of the BGA and fails again
once the BGA is released. It doesn't help that our board warps easily as
well. Is there anything, small gram weights or so that can weigh down a BGA
without shorting it?
Thanks
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|