Ron,
You may want to want to Rick Lathrop at Heraeus he may have a couple of
ideas that might help you.
Bev
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ron Peeler
Sent: Thursday, April 26, 2007 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Bev,
You are completely right. This product that I have been "baptized" into
has
been a 4 year terror. I am probably the 8th set of eyes to look at it.
I
have seemed to make the most progress but that doesn't mean a thing.
All I
do know is that the design is not good, the parts are obsolete and the
board
is already being produced in a new generation build, so basically I am
stuck
with what I have. Even though scrap is high on this board, they just
want
to pump them out till they fizzle out. So I am stuck with trying to
find a
reliable way to solder these BGA's when in 4 years they haven't been
able to
on this board. I know that the warping on the board is causing the
issue in
conjunction with the uneveness of the BGA package, neither of which can
be
changed.
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, April 25, 2007 4:58 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Ron,
The problem right now is you see an effect and you do not know the
cause. It could be that the board and/or component warps and you have
opens. It could be that you have a head-in-pillow situation. It could
be that you have internal component opens. It could be that you have
cracked solder joints. You have to figure out which it is before you
try to apply a remedy.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ron Peeler
Sent: Wednesday, April 25, 2007 4:38 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Don't try me I just might ask you that...
:)
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: Wayne Thayer [mailto:[log in to unmask]]
Sent: Wednesday, April 25, 2007 4:35 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Weights
Hi Ron!
I think most people solve this problem by making sure the board and BGA
are planar during the process, and that the solder paste is thick enough
to make up the difference. Then you have the "collapse" process working
for you too.
Weights can be used but are painful--last resort. They absorb heat,
messing up the solder profile, and need to be fixtured so they don't
fall off during reflow.
Next you are likely to ask for a rule of thumb for the pressure
supportable by the solder surface tension and the compression of the
solder balls which ensues. I don't know that--I just try weights until
it works.
Wayne Thayer
>>> [log in to unmask] 4/25/2007 4:23:12 pm >>>
Hello TechNet
I was wondering is there anything in the industry that is used to
weigh
BGA's down? We are having an issue @ our shop with BGA's not
soldering
effectively to one of our boards. Currently we have a board that is
suppose
to go through a boot process, however it has problems doing so. The
issue
is resolved when you press down in the middle of the BGA and fails
again
once the BGA is released. It doesn't help that our board warps easily
as
well. Is there anything, small gram weights or so that can weigh down
a BGA
without shorting it?
Thanks
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public
information. Any use of this information by anyone other than the
intended
recipient is prohibited. If you have received this transmission in
error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|