MS-810 - Guidelines for High Volume Microsection
Discusses the many variables and problems associated with the
process--from sample removal to micro-etch-- and the variables common to
high volume microsection. The process variables and problems are
organized so that the reader can research a specific issue or overview
the variables of a process area. 31 pages. Released October 1993.
Best regards,
Dave
David W. Bergman, CAE
Vice President, Standards, Technology and International Relations
IPC
3000 Lakeside Drive # 309S
Bannockburn, IL 60015
Phone 847-597-2840 Fax 847-615-5640
Mobile 847-867-1388
Main 847-615-7100
email [log in to unmask] www.ipc.org
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Clayton @
Reliability Resources
Sent: Monday, April 23, 2007 6:25 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-M-675
Mil Spec 810
Clayton Bonn
Reliability Resources
Ph: 714-903-1005
Cell: 714-612-9359
e-mail:[log in to unmask]
www.reliability-resources.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Monday, April 23, 2007 2:41 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-M-675
MS-810?
Rich K / GTS
847-621-7310
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Bergman
Sent: Wednesday, April 18, 2007 8:49 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-M-675
M-675 was an old IPC workshop handbook on microsectioning. 2.1.1 and
MS-810
are more up to date references.
Best regards,
Dave
David W. Bergman, CAE
Vice President, Standards, Technology and International Relations IPC
3000
Lakeside Drive # 309S Bannockburn, IL 60015 Phone 847-597-2840 Fax
847-615-5640 Mobile 847-867-1388 Main 847-615-7100
email [log in to unmask] www.ipc.org
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Mikell
Sent: Wednesday, April 18, 2007 2:50 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-M-675
The IPC website has a master list of standards, etc., listing their
revision.
<http://www.ipc.org/4.0_Knowledge/4.1_Standards/revstat1.htm>
That list has NO specification with 675 as its number or the letter "M"
as its classification.
Time to send the sacrificial lamb back to the customer for furthur
information.
Goog luck,
Steve Mikell
[log in to unmask]
----- Original Message -----
From: "Alistair Murray"
To: [log in to unmask]
Subject: [TN] IPC-M-675
Date: Wed, 18 Apr 2007 12:54:50 +0100
Hi to all
I am unable to find the above specification that has been referred to
me
by a customer. Can anyone help?
Thanks in anticipation
A Murray
Artetch Circuits
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET
Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet
Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|