When talking BGAs, has anyone tested the Sodiflux? Seems to be simple to use. The preheating/soldering by means of IR looks good. At least for single layer boards.
Inge
http://www.sodiflux.fr/fichier%20pdf/fritsch%20bga%20907.pdf
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Hfjord
Skickat: den 17 april 2007 19:39
Till: [log in to unmask]
Ämne: [TN] SV: [TN] Tacking corners of BGAs
Well then,
Work as distances. Why didn’t you say that from the beginning. Like we use sometimes: we remove some corner balls and replace with somewhat higher temperature. I understand now. Thanks.
Inge
-----Ursprungligt meddelande-----
Från: [log in to unmask] [mailto:[log in to unmask]]
Skickat: den 17 april 2007 19:10
Till: [log in to unmask]; [log in to unmask]
Ämne: Re: [TN] Tacking corners of BGAs
Hi Ingemar,
The corner epoxying serves not so much a mechanical fixation in the x/y-directions, but a way of preventing the solder balls from collapsing, and thus improving thermal cycling creep-fatigue reliability by (1) increasing h [with N h**2.2], and (2) improving the solder joint shape from squashed collapsed spherical to near-hour-glass. I also rather doubt that the 4 epoxy corners would be anywhere near strong enough to prevent the warping of superBGAs that thermally asymmetrically designed.
Regards,
Werner Engelmaier
可靠性先生
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************************************
See what's free at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|