One of our customers has asked us to look at changing the finish on a flex
circuit we manufacture from ENIG to Immersion Silver. The circuit is complex
and requires that we laminate on metal stiffeners after the immersion
silver. This would require a full cure cycle of approx. 375F for 1.25 hours
under pressure. The circuit would then have to undergo an approx. 6 hour
bake before assembly. Assembly requires 2 reflows. My question is will the
silver still solder. This is a Class 3 product and we are loading BGA's.
Thanks in advance. Steve Kelly
Steve Kelly
PFC Flexible Circuits Limited
PH: (416) 750-8433
Fax: (416) 750-0016
Cell: (416) 577-8433
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------