Thanks, Werner
Test condition B is 260C with the appropriate tolerances
Susan
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, April 18, 2007 2:13 PM
To: Susan Hott; [log in to unmask]
Subject: Re: [IPC-600-6012] Thermal Stress Testing for 6016 and 6012
Hi Susan,
I certainly would strongly lean towards IPC-6018 (HDI), para 3.6.1.
However, even this needs changing to 260°C.