Brian and Reuven,
Many aircraft materials are required these days to be "non-nutrient" or to
contain nothing that a fungus would consider to be food, thereby
encouraging growth. Some coatings go a step further by incorporating a
biocidal agent. I know that sometimes our units come back into the service
centers with green fuzzy layers growing on them from pilots spilling coffee
with cream and sugar, or sugared soft drinks, which gives the fungus (damn
spores are everywhere) something to feed upon. Having biocidal material
built in can be a more active defense against fungus growth.
Doug Pauls
Brian Ellis
<[log in to unmask]>
Sent by: TechNet To
<[log in to unmask]> [log in to unmask]
cc
04/10/2007 04:57 Subject
AM Re: [TN] Fongus treatment
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Brian Ellis
<[log in to unmask]>
Fungicides used to be added to phenol-formaldehyde lacquers, in the days
when all printed circuits were on cheap paper-based laminates (early
1950s, because the paper coating treater was poor in uniformity before
stacking prior to pressing. However, that was also in the days when
anode voltages were typically 250 V. I remember that 20 or so years ago,
some conformal coatings contained fungostats and bacteriostats, but I
haven't a clue whether they are still available. Normally, I would not
expect modern materials to support mycelia penetration, so fungostats or
fungicides should not be necessary. Beware that many fungicides are
based on ionic metal salts!
Brian
Reuven Rokah wrote:
>
> One of our potential customer is interesting with "Fungus treatment" for
> assemblies and cables.
>
> Do you familiar with such process?
>
> Thanks
>
> Reuven
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|