彭老师,您好!
谢谢您的答复!
有些引脚比较密的元件,比如贴片的连接器,如果客户强调上料时必须用烙铁手工焊接的话,我都要求操作员在显微镜下操作,因为这对焊接是有帮助的,但大部分元件如果用风枪上料的话我认为都不必在显微镜下操作,但焊接完成后肯定会要求在40X的显微镜检查。
所以我想了解的是IPC有没有具体规定什么类型的元件必须在显微镜下操作,什么样的元件推荐在显微镜下操作,而什么类型的元件不必在显微镜下操作,有个项目的客户要求我在WI里明确规定所有元件的返修都必须在显微镜下完成,而我认为这样反而回影响效率和焊接质量。
谢谢!
BR//ZHOU YIYONG
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Leesha Peng
Sent: Saturday, April 07, 2007 12:35 PM
To: [log in to unmask]
Subject: [TGA] 答复: [TGA]
Yiyong,
你好!
7711/7721中确实对用于返工维修的设备有要求.
1.8 工具和材料 印制板及组件的修改、维修、返工作业,一般是劳动密集型操作,更加依赖于操作者的技能。正确使用工具和材料对最终产品的功能和可靠性有着举足轻重的影响。为了使工作容易、提高成功机会,推荐下列设备和材料。仅作为参考。
1.完善的工作台 完善的工作台:ESD接地,适当的照明,方便人员进出,能提供舒适的坐姿更好,因为要想获得高可靠性的印制板及组件的修改、维修、返工作业,需要注意力高度集中、动作灵巧。
2.高质量的显微镜 精密作业一般都需要显微镜。参考IPC-OI-645标准了解关于目视光学检查辅助工具。
谢谢!
Leesha Peng 彭丽霞
标准开发/设计课程与技术资源部总监
Director, Standards/Design Programs
& Technical Resources
IPC WOFE, a subsidiary of IPC, Inc
上海市宜山路711号
Tel: 021-54973435
Fax: 021-54973437
手机:13902994705
________________________________
From: TGAsia 代表 Yiyong Zhou
Sent: 2007-4-2 (星期一) 19:51
To: [log in to unmask]
Subject: [TGA]
各位早上好!
有一个问题想请教一下,对于一些比较细小精密的元件,在做返修的时候有没有要求一定要在显微镜下操作,IPC在这方面有没有相关的要求和叙述?
谢谢!
BR//Zhou YY
Legal Disclaimer: The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
Legal Disclaimer:
The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
|
|
|