TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Date:
Mon, 9 Apr 2007 13:32:29 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Barmuta, Michael" <[log in to unmask]>
Subject:
From:
"Barmuta, Michael" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (204 lines)
Jim: The surface prep solution is a sodium-naphthalene based chemistry
designed to strip the Fluorine from the PTFE. If it is not applied
liberally enough it can not do its job. Because of the high cost of the
surface treatment chemistry people get stingy with the amount they use.
You need to submerge the board and work it across the surface. If you
are using it in air as opposed to a submersion tank with a nitrogen
blanket, you will need to add fresh solution for each board.

Once the board is treated give it two rinses in isopropyl alcohol i.e.
two tanks a dirty and a clean one. Follow this with two rinses in hot
water 120-140F. Same type of two tank set-up. This is necessary to
remove the residues of the treatment solution. 


	
Regards
	
Michael Barmuta
	
Staff Engineer
	
Fluke Corp.
	
Everett WA
	
425-446-6076

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James
Sent: Monday, April 09, 2007 11:48 AM
To: [log in to unmask]
Subject: Re: [TN] Water-break Test

So, you're suggesting etch the boards, water rinse, IPA rinse, acid
wash?  What type of mild acid would you suggest?  Do you need to D.I.
water rinse after the final acid wash?

Jim Marsico
EDO Corporation
Amityville:  631-630-5079
Bohemia:  631-218-7057
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Frederick Miller
Sent: Monday, April 09, 2007 3:40 PM
To: [log in to unmask]
Subject: Re: [TN] Water-break Test

I believe you need to use IPA as a first wash followed by a mild acid
wash. The supplier of the echant should be able to help.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of R Sedlak
Sent: Monday, April 09, 2007 1:32 PM
To: [log in to unmask]
Subject: Re: [TN] Water-break Test


Jim:

My suspicion is that it may well be impossible for you to get PTFE to
pass water break, certainly no cleaning/treatment after etch is going to
help.
The water break test is all about wetting, and PTFE is not going to wet
by water.  
That said, what is supposed to be happening with the sodium based etch,
is it is supposed to remove the Fluorine and thus convert the surface
into something else other than PTFE, presumeably more wettable.

I suggest that you take a test panel, and over-etch excessively.  It
could easily be that you are not etching enough.

Are you agitating during etching?   I suspect this would help.

Rudy Sedlak
RD Chemical Company

"Marsico, James" <[log in to unmask]> wrote: Hello Technet:

 

We have an application where we have to etch a PTFE PWB in preparation
for bonding.   The etch is a commercially available sodium-containing
solution.  We're also expected to meet a water-break test prior to
bonding.  We're having trouble meeting the water-break test and was
wondering if the two (etched PWB and water-break) are compatible.  If
so, what cleaning/rinsing could be performed after the etching to ensure
a water-break free surface?

 

Thanks in advance,

 

Jim Marsico

EDO Corporation

Amityville:  631-630-5079

Bohemia:  631-218-7057

[log in to unmask]

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


  
---------------------------------
Looking for earth-friendly autos? 
 Browse Top Cars by "Green Rating" at Yahoo! Autos' Green Center.  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2