TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 17 Apr 2007 13:45:54 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
In a message dated 4/17/07 13:39:24, [log in to unmask] writes:
> 
> Well then,  
>  Work as distances. Why didn’t you say that from the beginning. Like we use 
> sometimes: we remove some corner balls and replace with somewhat higher 
> temperature.  I understand now. Thanks.
> 
Hi Inge, given that we no longer have any "... somewhat higher temperature 
balls" in this crazy lead-free world of ours, this is a pretty neat solution.




Werner



**************************************