Hi Ingemar,
The corner epoxying serves not so much a mechanical fixation in the
x/y-directions, but a way of preventing the solder balls from collapsing, and thus
improving thermal cycling creep-fatigue reliability by (1) increasing h [with N
h**2.2], and (2) improving the solder joint shape from squashed collapsed
spherical to near-hour-glass. I also rather doubt that the 4 epoxy corners would
be anywhere near strong enough to prevent the warping of superBGAs that
thermally asymmetrically designed.
Regards,
Werner Engelmaier
可靠性先生
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************************************
See what's free at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|