TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
content-transfer-encoding:
7bit
Reply-To:
content-type:
text/plain; charset=us-ascii
Subject:
From:
Date:
Fri, 13 Apr 2007 10:22:55 +0530
Parts/Attachments:
text/plain (192 lines)
lee,
Can you provide us the paper you have mentioned in your mail for the barrel to copper.
Please provide me your mail id so that i can correspond with you on this further.
Thanks in advance for your reply.

Regards
suresh

Dehoyos, Ramon wrote at Thu Apr 12 18:04:28 GMT+05:30 2007:
> 
>	Lee:
>	Good to know info.  ^ current density, ^ brittleness,  v plating
>uniformity and density. Good things take time.
>	Thanks,
>	Ramon 
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
>Sent: Wednesday, April 11, 2007 12:42 PM
>To: [log in to unmask]
>Subject: Re: [TN] Via hole plating corner crack
>
>Victor
>
>You mentioned that the current density is 30 amps per square foot. I
>consider this to be extremely high and not only will cause brittle
>copper, but highly non-uniform copper in the barrel. I presented a paper
>at Apex that mathematically modeled the copper uniformity in the barrel
>to the plating parameters including current density, you might want to
>review this paper. The model shows there is an inverse linear dependence
>between the copper uniformity and the plating density.
>Best regards
>
>Lee
>
>J. Lee Parker, Ph.D.
>JLP Consultants LLC
>804 779 3389
>----- Original Message -----
>From: "Victor G. Hernandez" <[log in to unmask]>
>To: <[log in to unmask]>
>Sent: Tuesday, April 10, 2007 10:36 AM
>Subject: Re: [TN] Via hole plating corner crack
>
>
>   Can you please post the crack via cross section photo for viewing, "a
>picture is worth one thousands words".   Is this SnPb or LF?
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of C J Long
>Sent: Tuesday, April 10, 2007 9:20 AM
>To: [log in to unmask]
>Subject: [TN] Via hole plating corner crack
>
>Dear Techneter:
>
>I recently experienced customer return of corner crack. The PCB is 50
>mil
>thick, 10 mil via, OSP finish and corner crack is over the 4 corners of
>top
>and bottom
>of hole. Crack is started from the bottom of external foil and crack
>through
>
>the entire plating. You can see the photo (file: crack through) of
>actual
>failure. Plating is unusual column type crystal on the surface. In the
>hole
>barrel, the plating crystal is regular. We also performed many in-procss
>WIP
>
>cross section (refer to the file "crack 9X IR") and we could only find
>the
>crack after 6X IR reflow and its crack is started from external foil top
>corner. I have sucessfuly duplicated similar failire with very high
>plating
>current density of 30ASF with very low brighter (0.15cc/l), but its
>failure
>mode is crack on ehe top of external foil not the same as customer
>return.
> My questions are:
>
>1. Are these two failre modes with the same root cause? What is the
>reason
>one crack is started from the foil top corner and the other is from the
>bottom?
>2.Is there any non-destructive method able screening the cracked
>plating?
>
>
>http://tw.pg.photos.yahoo.com/ph/minalong2003/album?.dir=/5c32scd
>
>Thank you very much.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>for additional information, or contact Keach Sasamori at [log in to unmask]
>or 
>847-615-7100 ext.2815
>----------------------------------------------------- 
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>!-- Virus-Free Mail Using AntiVirus for IQ Mail & QuickHeal Engine --!
>



--
Thanks in advance for your reply.
Regards
T.Suresh Babu
Asst.Manager-Development.
Plot No.16,Jigani Indl Area,
Anekal Taluk
Micropack Ltd.,
Bangalore 562106
Ph-091-80-27825223/27826422
Fax:091-80-27825225
Email: [log in to unmask]


-------------------------------
Micropack Ltd, Bangalore, India


!-- Virus-Free Mail Using AntiVirus for IQ Mail & QuickHeal Engine --!

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2