Hi Al,
Is it wave soldering / manual soldering pads? Of through holes
components?
If yes, you should control the Alloy of the solder and the pre heating
and soldering temperature.
If it SMT components in reflow soldering, I do not have record of such
failure.
Reuven
e mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of al shirazi
Sent: Tuesday, April 10, 2007 7:56 PM
To: [log in to unmask]
Subject: [TN] pad lifting
Dear Techneter:
I recently experienced some failures and trying to understand why?
For SAC solder joints the pad lifting / Cratering happens to PCB
beneath the pad.
Can anyone think ways to prevent such failure from happening.
Thanks,
Al
---------------------------------
TV dinner still cooling?
Check out "Tonight's Picks" on Yahoo! TV.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|