TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Karl Hunsinger <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Karl Hunsinger <[log in to unmask]>
Date:
Fri, 27 Apr 2007 14:42:10 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (98 lines)
Our drawings almost always have a tolerance associated for vias. As Ramon just stated, we add a "plating factor" to the specified hole size to obtain the drill size. The expectation is to finish at the nominal (middle of the tolerance) hole size.

Karl

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dehoyos, Ramon
Sent: Friday, April 27, 2007 2:32 PM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"


Agreed, We just went through such an exercise and the conclusion
was that the specified hole size was the final hole size. A 6, 7, 8 or 5
mils were added to find the drill size.
Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Smith, Richard
Sent: Friday, April 27, 2007 10:05 AM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"

I don't disagree but, unless I'm behind the times which is entirely
possible, the IPC used to promote the practice of specifying all plated
hole sizes as finished permitting the manufacturer to select the
appropriate drill. I'm not implying this is the best practice, but on
the other hand I've not seen a via reliability issue attributable to the
finished via hole tolerance on the drawing.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Thursday, April 26, 2007 3:23 PM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"

Hi All,
Vias should never be specified in terms of finished hole size (there is
no
functional need for any specific finished hole diameter), but in terms
of
drilled hile diameter, because that determines all kinds of things
important to the reliability of the via interconnect structure.

Werner



**************************************
 See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2