Our customer is questioning what they feel is exposed copper in 8 mil vias
holes on silver boards. We feel there is mask residue in the holes which does
not allow silver to take. These are holes that are allowed to be plugged. Has
anyone else ran into this issue with thier customers and do you have the same
look or are your small vias covered with silver all the way through the via?
---------------------------------------------------