It's not advisable to repair type AR conformal coating with type UR.
The solvent from the type UR will usually dissolve the acrylic.
Mixtures of types AR and UR conformal coatings do not have MIL SPEC approval. They have never been tested. I have literally seen thousands of conformal coating candidiates fail those tests. It would be like using an unapproved coating.
It is likely that acrylic would interfere with the polyurethane curing.
The interface of the resultant coating would be of variable composition.
To go one step further we did not recommend repairing 1B31 with type 1B73 and visa vera.
The combination was never been tested. There are ways of distinguishing between the 2 coatings.
Ed Mines
---------------------------------
We won't tell. Get more on shows you hate to love
(and love to hate): Yahoo! TV's Guilty Pleasures list.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------