Hi all...
I've done a handful of space flight type PCB layouts that
used 1812's as a minimum. This is because NASA worries about whiskers
forming
between the metal plates.
Ken
__________________________________________
Kenneth Wood
Saturn PCB Design, Inc.
2737 Bishop Lane
Deltona, Fl 32725
Phone: 407-275-3220
Email: [log in to unmask]
Internet: http://www.saturnpcb.com
_________________________________________
-----Original Message-----
From: Bloomquist, Ken [mailto:[log in to unmask]]
Sent: Friday, March 16, 2007 10:49 AM
To: [log in to unmask]
Subject: [TN] Engineering Question
Since it's Friday this could be a joke but I don't really think so.
Design Engineering asked Manufacturing Engineering, (believe it or not), "Do
you have any guidance on the maximum size we want to use for ceramic SMT
caps?"
I believe their concern is coming from the potential for cracks during
processing. We currently and probably will for quite some time use SN63 for
all our processing so the higher temperatures are not an issue.
Any guidance would be appreciated,
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--------------------------------------------------------------------------------
This email and any files transmitted with it are intended only for the use of
the individual or entity to which it is addressed and may contain information
that is proprietary, confidential and exempt from disclosure under applicable
law. If the reader of this message is not the intended recipient, or the
employee or agent responsible for delivering the message to the intended
recipient, you are hereby notified that any dissemination, distribution or
copying of this communication is strictly prohibited. If you have received this
communication in error, please delete it and notify us immediately.
--------------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|