I saw your question and meant to read the spec before answering, but finding
the time to read the spec..... Anyway I still haven't refreshed on the spec
so off the top of my head I would rationalise as follows:
The impurities on supply are listed to ensure high quality. Not everything
is listed just those things that are likely to be there which if present in
excessive amounts would be detrimental or indicative of poor quality raw
material. Indium would fall into the likely to be there category.
The impurities listed in use are those which would increase as a
consequence of use and which could have a detrimental effect on performance
and thus require to have a guidance on acceptable amounts.
So it is quite possible to have an impurity in the as supplied list but not
in the in use list.
Indium will not increase during use as it would not be present to wash off
boards/ component terminations. However even if were present and did
accumulate in pot, it would have to increase enough to effectively be a
significant alloying addition before it changed solder properties. This is
unlikely in the extreme so therefore no need to list it.
When reading specs keep in mind that they don't usually get written from
scratch on to a clean sheet. Those with a long lineage - and solder specs go
back to before electronics - they are usually the result of a long series of
hand me downs and other bits joined on later, so probably do end up with
some apparently contradictions which made sense at the time but when read
together in the new context clunk a little.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
---------------------
Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence)
77-97 Harpur Street, Bedford , UK
Registered number: fc16473
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Thursday, March 15, 2007 1:03 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Purity
Brian:
It seems that there this is an oversight by the IPC. I
have found other inconsistencies and have forwarded them to IPC. Feel
free to let them know since you were the one that made the observation.
Some times people do not respond, because the ones that can make
comments on difficult subjects like this, are really busy and do not
check the TechNet list.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, March 15, 2007 8:40 AM
To: [log in to unmask]
Subject: [TN] Solder Purity
Good morning,
A little over a week ago I posed a question regarding solder
purity
and a perception of conflict between J-STD 001 & J-STD 006. Luck was
not
with me as there were no replies. Alas, I will try one more time in
hopes that the tech gurus here can provide some insight or solutions
based on similar experience.
Previous post:
I am hoping that someone can help us with a clarification regarding
solder purity/composition requirements. Specifically the following:
ANSI J STD 006 on page 3 lists allowable impurities in the solder
alloy
when purchased. One component in particular is indium @ 0.10
allowable
limit.
However, ANSI J STD 001 which is the assembly specification used in
daily production lists on page 5 allowable solder impurities which
does
not include/allow Indium.
ANSI J STD 001 which is also the specification used for testing lists
on
page 5 allowable solder impurities which also does not allow Indium.
Perhaps we are interpreting the sentence associated with the table on
both 001 and 003 wrong, however the sentence does state: "the
balance
of the bath shall be lead and/or the items listed above." How can you
allow Indium in the raw purchased solder and not allow it in the
production solder?
Thank you in advance for your thoughts and clarifications.
Brian Guidi
Senior Product Engineer / N.P.I.
Teledyne Printed Circuit Technology
Tel: (603) 889-6191 X:310
Fax: (603) 886-2977
E-mail: [log in to unmask]
Visit us @ http://www.tetpct.com
Any technical information attached to this document is intended for the
recipient only. Also, the export and use of the information is
regulated by the export laws of the United States. Diversion contrary
to U.S. law is prohibited. U.S. law prohibits sharing this information
with any end-user for any end-use related to the design, development,
production, stockpiling or use of chemical, biological or nuclear
weapons or missiles, without the prior approval of the United States
Government.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|