Hi Dave,
It is quite a bbit more involved than just T260, or T288 or T300 for that
matter. That is one of the reasons I developed the STII-concept, which while
great for an initial selection approach, also does not address all the needed
issues for successful lead-free assembly.
That is why I have developed my White Paper: "Recommendations for PCB FAB
Notes and Specifications in Printed Circuit Board Drawings for SnPb and Lead-Free
Soldering Assemblies, the Qualification of PCB Shops and Activities to Assure
Continued Quality."
Regards,
Werner Engelmaier
可靠性先生
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************************************
AOL now offers free email to everyone. Find out more about
what's free from AOL at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|