Given the nature of the finishes, and their relative low hardness
(certainly in the case of lead free HASL) you probably would be able to
use a device called a Shore Schleroscope, which in principle is a
pen-like device with a ball bearing which drops onto the surface being
measured. The amount of "bounce" detected determines the surface
hardness of the finish.
I would suspect that the amount of area being measured would have an
influence, so it may be best to organise a series of base test panels
which are identical for all the proposed finishes.
There are several other types of measuring, dependant on the hardness of
materials tested (Steel can be measured by an Izod impact test etc) and
various conversion charts which will give conversions into Rockwell,
Knoop values etc.
Hope this helps
Colin W.T. McVean M.Inst.C.T
Production Manager
Artetch Circuits Ltd (www.artetch.co.uk)
Direct Dial 01903 712926
Switch Board 01903 725365
Skype: colin.artetch
P Before printing , please think about the Environment
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of arnaud grivon
Sent: 23 March 2007 10:19
To: [log in to unmask]
Subject: [TN] Hardness Characterization of a PCB Surface Finish
Hello TechNet,
What would be the adequate technique(s) to characterize the hardness of
a given PCB surface finish (resistance to electrical test probe impact)?
Concerns are varying marks of electrical test probes after assembly
depending on the PCB source.
Regards,
A. Grivon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|