DESIGNERCOUNCIL Archives

March 2007

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Anderson, Suzanne" <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Wed, 14 Mar 2007 13:17:28 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (213 lines)
Bill,

      Would the plugged via be conducive to ICT if the Test Pads were
vias? Would it lead to false opens?

Regards,

Suzanne

 

Suzanne Anderson CID+

Kollsman, Inc.

220 Daniel Webster Hwy.

Merrimack, NH 03054

Email: [log in to unmask]

Phone: 603-886-2290

 

 

-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Brooks,Bill
Sent: Wednesday, March 14, 2007 12:55 PM
To: [log in to unmask]
Subject: Re: [DC] One sided issue

 

Let me see if I understand the implied issue... 

 

If they are tenting the vias on one side I would suggest recommending

another more reliable option to your customer. 

 

We plug the vias with soldermask here rather than 'tent' them for a
couple

of reasons... one, a single sided or broken tent is a moisture or
chemical

trap and can compromise or damage the board or assembly during assembly

processing or even in storage. 

 

Two, from my own experience, we had a batch of tented boards make it
into

assembly with compromised tents, (ones that did not completely cover the

holes on either side) and when we ran the boards through re-flow
soldering

we observed in inspection a large number of the vias expelling solder
balls

and contaminants from the holes as the heated gasses and moisture inside

them expanded rapidly... (Kind of like little volcanoes)...  

 

We avoid the single sided tents for that exact reason... 

Plugging the holes completely is much more reliable and we have not had
any

problems since.

 

Does that help at all?

 

 

Best regards,

 

Bill Brooks 

PCB Design Engineer, C.I.D.+

Tel: (760)597-1500 Fax: (760)597-1510

Datron World Communications, Inc.

Vista, California

 

-----Original Message-----

From: Brad Saunders [mailto:[log in to unmask]] 

Sent: Tuesday, March 13, 2007 2:02 PM

To: [log in to unmask]

Subject: [DC] One sided issue

 

Hello Folks,

What are the reliability thoughts on a PCB configuration as follows: 013
PTH

via ENIG finish (prior to soldermask) with one side without mask and the

other a dryfilm soldermask.  The board is approx .080 thick.

Thanks, Brad

 

------------------------------------------------------------------------
----

-----

DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV

1.8d

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF DesignerCouncil.

To temporarily stop/(restart) delivery of DesignerCouncil send: SET

DesignerCouncil NOMAIL/(MAIL)

Search previous postings at: www.ipc.org > On-Line Resources & Databases
>

E-mail Archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16

for additional information, or contact Keach Sasamori at [log in to unmask]
or

847-615-7100 ext.2815

------------------------------------------------------------------------
----

-----

 

------------------------------------------------------------------------
---------

DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF DesignerCouncil.

To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)

Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

------------------------------------------------------------------------
---------


_______________________________________________________________________
This e-mail message has been sent by Kollsman, Inc. and is for the use
of the intended recipients only. The message may contain privileged
or confidential information. If you are not the intended recipient
you are hereby notified that any use, distribution or copying of
this communication is strictly prohibited, and you are requested to
delete the e-mail and any attachments and notify the sender immediately.

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2