Happy Friday Jim! This is only a guess but one possible reason for such a
recommendation is the potential to have solder joint integrity degradation
due to gold embrittlement. A high tin content solder alloy and gold surface
finishes do not necessarily mean a gold embrittlement situation but it
would be on aspect of a solder process that would need to be kept in mind.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Marsico, James"
<James.Marsico@ED
OCORP.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
03/30/2007 06:46 [TN] Soldering using Sn96
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Marsico, James"
<James.Marsico@ED
OCORP.COM>
Technetters:
I happened to come across a solder chart from the Indium Corporation and
noticed that they do not recommend using Sn96 solder on gold-plated
surfaces. Can anyone elaborate on this?
Jim Marsico
EDO Corporation
1250 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------