free ads for cmap... Must be paid more than a penny...
By the way, the old penny is copper alloy... But the non-copper elements
increased after 1960...you can tell from the grain size if you care to dip
the penny into yoyur wife's Javex bleach (diluted HCl I think)...for some
time...The new penny got finer grain compare to the old one...Have a nice
weekend...
abcd
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hernefjord Ingemar
Sent: Friday, March 09, 2007 8:46 AM
To: [log in to unmask]
Subject: Re: [TN] copper deterioration (NTC?)
Brian, you must wonder a lot. In fact, I copied wrong site adress, here
is a more correct one, even if CAF is also of interest.
http://www.money.org/Content/NavigationMenu/ExploretheWorldofMoney/FAQs/
us_coins_faq.htm
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: den 9 mars 2007 13:25
To: [log in to unmask]
Subject: Re: [TN] copper deterioration (NTC?)
One penny can be enough to live on for the rest of your life, Brian.
Don't?
Look here:
http://www.cmap.ca/open/events/2002May_Reliability/presentations/Turbini
%20CAF.pdf
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: den 9 mars 2007 13:17
To: [log in to unmask]
Subject: Re: [TN] copper deterioration (NTC?)
I thought (a penny's worth) the modern ones were in zinc, thinly
copper-clad, because solid copper would be worth more than 1 cent in
intrinsic value. As it is, I think the cost of manufacture is higher
than 1 cent (if that is not true, does it become a mint humbug?).
Brian
Louis Hart wrote:
> TechNettters, not sure if this is a true NTC, but after looking at the
> postings about exposed copper, it occurred to me that the US one-cent
> coin is made of what I think is a predominantly copper material not
> likely to be an expensive superalloy. Whenever I get one made in the
> 1950s, it still shows has plenty of sculptural detail. Lou
>
> Louis Hart
> Technology Transfer Specialist
> National Technology Transfer Center
> 316 Washington Av
> Wheeling, WV 26003
> 304-243-2553
> [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|